Armored figure
A crowned head and pointed shoulders rise above long robes and a round base.
Rigid models with a short water-cleaning step
Contact for pricing
1 kg · White · Quantity 1
Select color and pack
Color White
The supplier specifies water washing for up to 3 minutes; prolonged soaking can damage the part.
Listed 200–300 cP at 25°C supports a flow-focused material comparison.
Positioned for display models, figures and toys; test the intended fine features and finish.
A crowned head and pointed shoulders rise above long robes and a round base.
Layered feathers, talons and a curved tail surround a textured terrain base.
Three separate head components retain their supports and printing rafts.
The full figure includes both held items and boots; the source view remains small.

An umbrella and cat sit above a torii-inspired structure and fish-shaped base.
A hand holds the architectural ruin in its original photographed setting.
| Property | Value |
|---|---|
| Shore hardness | 80D |
| Viscosity at 25°C | 200–300 cP |
| Tensile strength | 47.6 MPa |
| Elongation at break | 3.5% |
| Material wavelength | 365–405 nm |
| Curing time(s) | 2–4 s |
| Shelf life | 1 year |
Supplier-listed starting reference for a 10.1-inch 8K test machine, with light intensity printed as 5,000 µW/cm². Calibrate on the intended printer and batch.
| Setting | Reference values |
|---|---|
| Working temperature | 20–35°C |
| Layer height | 0.05 mm |
| First-layer exposure | 20–30 s |
| Exposure time | 1.5–3 s |
| Setting | Reference values |
|---|---|
| Rest / light-off after return | >1 s |
| Lift · LCD screen <8.9 inches | 5 mm |
| Lift · LCD screen ≥8.9 inches | ≥7 mm |
The bottle label gives separate starting values for monochrome and color screens at 0.05 mm layers.
| Setting | Bottle-label reference |
|---|---|
| Monochrome screen · 0.05 mm · exposure | 2–3 s |
| Color screen · 0.05 mm · exposure | 5–10 s |
| Monochrome screen · 0.05 mm · bottom exposure | 20–30 s |
| Color screen · 0.05 mm · bottom exposure | 40–60 s |
Shake before pouring. Clean the vat and build plate, keep the vat bottom clear and choose the correct resin settings.
Use the printing references above with their listed conditions, then calibrate the actual printer, layer height and batch.
Use a scraper to separate the part from the build plate. Work carefully around supported and delicate features.
Wash in water for no more than 3 minutes. Avoid prolonged immersion: the supplier warns that a 24-hour soak can soften or crack parts. Use protective gloves and avoid skin contact with uncured resin. Collect resin-contaminated wash liquid for appropriate disposal; water washing does not make waste suitable for a drain. Equipment photographs show the external process and do not establish compatibility or cycle settings.
Blow dry promptly after washing; the supplier names a high-pressure air gun but gives no pressure, temperature or duration. Choose a controlled method for delicate details.
The supplier lists 2–5 minutes with a 385–405 nm UV source of approximately 40 W. Check the cycle on your part.
Inspect support marks, detail and fit before use. Seal resin away from light, heat, dust and moisture. The supplier lists storage at 25–35°C; this is distinct from the 20–35°C working reference.
Start with the supplier settings above and calibrate for your printer and resin batch.
The supplier specifies a short cleaning step and warns that 24-hour immersion can soften or crack parts. Water-cleanable does not mean prolonged water exposure is qualified.
No. Application photographs illustrate the visible geometry and development task. Confirm the actual supplied color and surface on a sample.
Model size, fine features, water-cleaning method, drying arrangement and printer.
Share your part dimensions, wall thickness, printer and required surface finish.
Choose your color, pack size and quantity above to prepare your enquiry. Add project details in the enquiry form.
Choose your options ↑